玻璃微珠生產(chǎn)設(shè)備基礎(chǔ)知識
玻璃微珠生產(chǎn)工藝是火焰漂浮法,主要運用到兩個系統(tǒng),一個是懸浮加熱融化,一個是冷卻成型。玻璃微珠生產(chǎn)流程:1、原料粉碎:將廢舊玻璃粉碎成相應(yīng)大小的玻璃砂;2、生產(chǎn)燒制:將玻璃砂在懸浮爐中用天然氣燒制成型,然后冷卻掉落至成品收集器中;3、篩分包裝:將制半成品玻璃微珠按照相應(yīng)粒徑大小篩分打包;
Machine Type |
DR-SAU-21-15 |
Raw Material |
Plate Glass |
Max Weight ofRaw Material |
3 Ton per Furnace per 5 Hour |
Final Product Standard |
According to AASHTO BS MOT Std |
Staff for the total Line |
4 Person For Crusher(8 Hour)--Total 4 2 Person per shift for Furnace(8 Hour)-Total 6 5 Person for Sieve and Packing(8 Hour)--Total 5
|
ProductionCapacity Per Day |
14 TON per Furnace per 24 Hour |
Site Required For Total Line (L*W*H) |
20M*8M*17M |
Size of the Furnace |
Φ900mm*10000mm |
Temperature of Furnace |
950-1100℃ |
Structure For the Line |
Steel welded framework |
Spec of Burner |
18PCS Size:100mm*3700mm |
Color |
Per client’s requirements |
Electric Cabinet |
3 units |
Power Supply |
380V,60Hz,3 Phase; |
Pressure of Gas |
≥100KPa |
WaterSupply |
Temperature ≤35°C 20Ton Per 24 hour PerFurnace |
Gas |
450-550m3PerHour PerFurnace |